Layer-by-layer coating with alginate, chitosan and MGF inhibited the degradation rate of ZEK100 samples in vitro and in vivo.
In plain wordsIn lab tests and in animals, the coating slowed the breakdown of the metal alloy.
- Peptide
- MGF / PEG-MGF
- Outcome
- DecreaseDegradation rate of coated alloy in vitro and in vivo
- Study
n: not reported in source
ZEK100 magnesium alloy implant, in vitro and in vivo (femur medullary cavity)- Comparator
- Uncoated ZEK100
- Outcome group
- Bone and joint · Musculoskeletal
Source sentences
By comparing the degradation of uncoated and multilayer-coated ZEK100 samples in vitro and in vivo, respectively, it is found that the degradation rate of ZEK100 samples can be inhibited by LBL modification on the surface of the sample
1 context sentence(design, population, supporting numbers)
Fabrications of multilayered coatings carrying sodium alginate (ALG), chitosan (CHI) and mechano-growth factor (MGF) on fluoride-pretreated ZEK100 magnesium alloy have been obtained via layer by layer (LBL) to reduce the degradation rate of magnesium alloy in this study.
In this study, MGF / PEG-MGF was a lab tool or a carrier, part of a mix, or the subject of a lab method. This result is not evidence about taking MGF / PEG-MGF.